Abstract
Diamondlike thin films were prepared by irradiation of high purity graphite with a high power density( 1.178 x I 09 Watt I cm2 ) laser (XeCI 308 nm) in the vacuum ( I x 10-s Torr) . Raman spectra show the thin film with the properties of diamond, the scatter peak is in round 1330 cm-1 . The IR spectra show the thin film containing C-H bonds, and the ratio ofH to C is about 45%. The resistivity and optical energy gap of the thin film are 1.89 x 106 .0 .cm and 1.55 e. V, respectively. Keywords: Pulsed Laser deposition, Diamondlike thin film, Raman spectra.
© (1998) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
You-qing Wang, Qiulang Wang, Chengwu An, and Biao Su "Pulsed laser scanning deposition of diamondlike thin films", Proc. SPIE 3175, Third International Conference on Thin Film Physics and Applications, (20 February 1998); https://doi.org/10.1117/12.300671
Lens.org Logo
CITATIONS
Cited by 1 scholarly publication.
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Laser scanners

Thin film deposition

Thin films

RELATED CONTENT


Back to Top