The investigated Bragg fiber consisted of the 26um diameter silica core surrounded by three pairs of circular Bragg layers. Each pair is composed of one layer with a high and one layer with a low refractive index being characterized by a refractive-index contrast up to ~0.03. The 1064nm laser beam was focused by a telescope onto the fiber input face. The beam radius in the focal plane was 5um. The Bragg fiber output face was imaged by a 1:6 optical telescope on the CCD camera. The transmitted power and spatial beam profile were registered simultaneously for various offset from the fiber axis. After the fiber shortening, the measurement was repeated and the cut-back was performed. The lowest attenuation coefficient of 0.17dB/m corresponded to a core mode of the delivered laser radiation. In general, the attenuation was higher with a shift from the radial axis of the fiber symmetry. In the case of cladding mode excitation, the attenuation parameter shows a local minimum. This phenomenon was consistent with the refractive index profile of the tested Bragg fiber. |
ACCESS THE FULL ARTICLE
No SPIE Account? Create one
Signal attenuation
Cladding
Refractive index
Optical fibers
CCD cameras
Transmittance
Modes of laser operation