22 April 2005 Hydroxyapatite kinetic deposition on solid substrates induced by laser-liquid-solid interaction
Liliana Pramatarova, Emilia Pecheva, Todor Petrov, Radina Presker, Martin Stutzmann
Author Affiliations +
Proceedings Volume 5830, 13th International School on Quantum Electronics: Laser Physics and Applications; (2005) https://doi.org/10.1117/12.619002
Event: 13th International School on Quantum Electronics: Laser Physics and Applications, 2004, Bourgas, Bulgaria
Abstract
Hydroxyapatite (HA) is present in the human body as a mineral constituent of the bones and teeth, as well as a major or minor component of kidney stones. HA deposited on different solid substrates can find applications including biomaterials and biosensors. This work deals with the kinetics of the HA growth by applying a novel method of laser-liquid-solid-interaction (LLSI) process on three types of materials (stainless stell, silicon and silica glass). The method allows interaction between a pulsed laser and a substrate immersed in a solution (simulated body fluid, SBF). By a scanning system, a design of seven squares at a distance of 200 μm was created at the end of each sample. In this way the center of the substrate (about 6x6 mm) was no irradiated. Following the LLSI process, the samples were left in the irradiated SBF for various intervals of time. Light microscopy (LM) showed surfaces seede with randomly distributed transparent and white particles. The surface seeding increased with the immersion time and was dependent on the substrate type. Fourier transform infrared (FTIR) spectrsocopy showed that in the first stage of soaking (up to 6 h) the observed white particles were calcium phosphate containing. Energy dispersive X-ray (EDX) spectrsocopy revealed that the transparent particles were NaCl. In the next stage (after 12 h) vibrational modes typical for HA were clearly observed. Detailed observation with scanning electron microscopy (SEM) after 12 h showed morphology of sphere-like aggregates, grouped in a porous network. Raman spectroscopy, X-ray diffraction (XRD) and EDX confirmed that after 12 h the grown layer was HA. It was found that in comparison to the traditionally empoyed prolonged soaking in SBF, the applied LLSI process yielded a synergistic effect due to the simultaneous use of the solid substrate, the aqueous solution and the laser energy.
© (2005) COPYRIGHT Society of Photo-Optical Instrumentation Engineers (SPIE). Downloading of the abstract is permitted for personal use only.
Liliana Pramatarova, Emilia Pecheva, Todor Petrov, Radina Presker, and Martin Stutzmann "Hydroxyapatite kinetic deposition on solid substrates induced by laser-liquid-solid interaction", Proc. SPIE 5830, 13th International School on Quantum Electronics: Laser Physics and Applications, (22 April 2005); https://doi.org/10.1117/12.619002
Lens.org Logo
CITATIONS
Cited by 2 scholarly publications.
Advertisement
Advertisement
RIGHTS & PERMISSIONS
Get copyright permission  Get copyright permission on Copyright Marketplace
KEYWORDS
Solids

Bone

FT-IR spectroscopy

Laser irradiation

Particles

Pulsed laser operation

Seaborgium

Back to Top