Carbon Fiber Reinforced 1Plastic (CFRTS) and TC4 titanium alloy have excellent properties such as high stiffness, fatigue resistance and corrosion resistance, which are widely used in aerospace and new energy vehicle manufacturing. Due to the great differences in physical and chemical properties between CFRTS and TC4 titanium alloy, the traditional bonding and riveting methods have the problems of aging and stress concentration. This study introduces the interface composite control process of “picosecond laser cleaning and plastic-covered”. Firstly, CFRTS was subjected to laser cleaning pretreatment to remove the surface epoxy resin. Secondly, laser was used to pretreat the surface microstructure of TC4 titanium alloy. A layer of 0.02 mm PA powder was spread on the surface of the microstructure and melted by laser to form a plastic-covered layer. Finally, the treated CFRTS and TC4 titanium alloys were welded by laser-assisted joining. Compared with the traditional cleaning technology, it was found that the carbon fiber was exposed obviously and the structure was complete on the CFRTS surface after picosecond laser cleaning, and the epoxy resin was removed completely. The porosity of the joint interface is reduced, and the weld morphology is better. The shear strength of CFRTS-TC4 titanium alloy joint is significantly enhanced, and the maximum shear strength is 6333 N.
Laser additive manufacturing (LAM) is a novel technology that uses high-energy laser beam to obtain high performance entities and coatings. However, in this process, it is difficult to control the microstructure of materials effectively by changing the laser parameters. Based on this situation, we proposed a method that using direct electrostatic field (DESF) to assist LAM process. In this paper, we investigated the changes in 316L microstructure after assisted by DESF, and discuss the effect of electrostatic field. Microstructures of the 316L stainless steel sample fabricated by this method were tested. The result showed the solidification direction and grain morphology was influenced by the direction and value of DESF obviously. While the ESF direction is opposite to the laser scanning direction, the grains in the longitudinal-section perform orderly growth and the directions are biased to the laser scanning direction. While the DESF direction is the same as the scanning direction, the original solidification direction is obviously changed and the direction tended to be opposite to the scanning direction.
With the lightening tendency in the automobile and aircraft industry, the aluminium (Al) alloy and the carbon fiber reinforced thermal polymer (CFRTP) has been widely used. The CFRTP component always needs to be joined with Al alloy to form a CFRTP/Al alloy composite structure. Due to the large differences in the physicochemical properties of CFRTP and Al alloy materials, it is difficult to join with each other. Laser stir welding technology was applied to join CFRTP and Al alloy dissimilar materials in this research. In order to improve the CFRTP/Al alloy joining strength, a surface pre-treating method (laser micro-engraving) was proposed in this paper. Three micro-scale structures were designed and prepared on 7075 Al alloy by surface laser micro-treatment, which are linear grooves, mesh grooves and circular grooves. The morphology and dimensions (width and depth) of the microstructure on the strength of CFRTP / Al alloy joints were studied. The interface morphology and the fracture morphology of the joint were observed by the laser confocal microscopy and the scanning electron microscopy (SEM). Furthermore, the joining mechanism and failure mechanism of the CFRTP/Al alloy joint were explored. The results indicated that the microscale structures play an important role in improving the mechanical properties of Al alloy and CFRTP joins under different laser micro-engraving.
AlCrFeMnNi high-entropy alloy was prepared by laser additive manufacturing with gas-atomized pre-alloy powders. The phase, microstructure and microhardness of HEA have been investigated. The HEAs without electric field controlled and under controlled were composed of single BCC phase. Under the controlling of electric field, the pores presented the phenomenon of reducing. Due to the reducing of pores, the HEA under electric field controlled became harder and exhibited high microhardness of about 529.9 HV0.2, which was 6.49% higher than the HEA without controlled.
Access to the requested content is limited to institutions that have purchased or subscribe to SPIE eBooks.
You are receiving this notice because your organization may not have SPIE eBooks access.*
*Shibboleth/Open Athens users─please
sign in
to access your institution's subscriptions.
To obtain this item, you may purchase the complete book in print or electronic format on
SPIE.org.
INSTITUTIONAL Select your institution to access the SPIE Digital Library.
PERSONAL Sign in with your SPIE account to access your personal subscriptions or to use specific features such as save to my library, sign up for alerts, save searches, etc.